Overview
Section 1 - Mix
User
FalconProject
Type1
Hybrid Binder
Type2
Others
Mix ID
161
Materials
Material
Weight g (%)
Material Family
Commercial Name
Price
True Density
Bulk Density (g/cc)

Water
225 (11.11 %)
Water

Standard sand
1350 (66.67 %)
Fine Aggregate

Cement 52.5N
88.37 (4.36 %)
Portland Cement

FALCON slag
173.18 (8.55 %)
Industrial Slag / Glass
3.17

Argical 1200S
19.52 (0.96 %)
Mineral

Gypsum
72.81 (3.60 %)
Mineral

Fly ash class F-example
61.04 (3.01 %)
Ash

Limestone powder
32.59 (1.61 %)
Mineral

Gypsum
2.49 (0.12 %)
Mineral

Placing & Curing
Shaping
De-Airing
Curing conditions
Duration (Mins)
Conditions after curing
Duration (Mins)

Casting
Jolting
Other

Hardened Properties
Standard (Mortar)
Standard (Concrete)
Value
Standard Deviation

-
-
5.69807
-

-
-
13.0041
-

-
-
5.84504
-

Others
Standard (Mortar)
Standard (Concrete)
Value
Standard Deviation

-
-
88.0598
-