Overview
Section 1 - Mix
User
Lubi
Type1
Hybrid Binder
Type2
Hybrid Binder
Mix ID
62
Materials
Material
Weight g (%)
Material Family
Commercial Name
Price
True Density
Bulk Density (g/cc)

Georis steel slag mix
315 (15.56 %)
Industrial Slag / Glass

Cement 52.5N
135 (6.67 %)
Portland Cement

Sand
1350 (66.67 %)
Coarse Aggregate

3M NaOH
225 (11.11 %)
Other Component

Placing & Curing
Shaping
De-Airing
Curing conditions
Duration (Mins)
Conditions after curing
Duration (Mins)

Casting
Jolting
20-22°C & 60-70% Humidity

28

Hardened Properties
Standard (Mortar)
Standard (Concrete)
Value
Standard Deviation

-
-
2.4
-

-
-
2.79
0.05