Showing 101-103 of 103 items.
Sustainable Resources Database
SREWay code | Uploaded by | Name | Information | Location | Source | Status | Category | Resource Category | Chemical Composition | Elements | Actions |
---|---|---|---|---|---|---|---|---|---|---|---|
65 | jorn | (FeO)0.71(SiO2)1(CaO)0.52(Al2O3)0.1 | Synthetic slag SA2 | KU Leuven Department of Materials Engineering, Leuven, Belgium | Jorn Van De Sande | Laboratory Slag / Glass | Not available / Not listed / Not available / Not listed / Not available / Not listed (EEA code: 999.999.999) | SiO2 - 39.9 wt% FeO - 34.1 wt% CaO - 19.3 wt% Al2O3 - 6.5 wt% Others: 0.2 wt% | Al Ca Fe Si | View | |
112 | Giels | Vitrified red mud - 1st pilot trial | This material is the result of a first pilot trial in RWTH Aachen, where red mud is molten with additives at 1250 - 1300 °C. After quenching a semi glassy precursor is obtained with high reactivity. | KU Leuven | Michiel Giels | Industrial Slag / Glass | WASTES FROM INORGANIC CHEMICAL PROCESSES / Not available / Not listed / Not available / Not listed (EEA code: 06.999.999) | FeO - 34.5 wt% Al2O3 - 18.5 wt% CaO - 18.5 wt% SiO2 - 17.6 wt% Na2O - 6.9 wt% TiO2 - 2.8 wt% Others: 1.2 wt% | Al Ca Fe Na Si Ti | View | |
140 | YiannisPon | Trial activating solution; H2O is 90wt% | Alkali-silicate | Not available / Not listed / Not available / Not listed / Not available / Not listed (EEA code: 999.999.999) | SiO2 - 61.5 wt% Na2O - 38.5 wt% | Na Si | View |